Official Journal of the Japan Wood Research Society
Treatment with RR | Leaching | WLterm (%) | TSR (%) | VS | |
---|---|---|---|---|---|
Control samples | No EtOH | No | 11.2 ± 1.4 | 71.6 ± 13.4 | 4 |
With EtOH | No | 14.0 ± 2.3 | 76.3 ± 8.9 | 4 | |
RR (1%)/EtOH (99%) | No | 9.0 ± 1.0 | 57.3 ± 4.6 | 4 | |
Yes | 11.4 ± 1.9 | 70.0 ± 5.3 | 4 | ||
RR (5%)/EtOH (95%) | No | 2.7 ± 0.0 | 2.0 ± 3.5 | 1 | |
Treated samples | Yes | 8.6 ± 0.9 | 48.7 ± 19.0 | 4 | |
RR (10%)/EtOH (90%) | No | 2.5 ± 1.3 | 2.0 ± 3.5 | 1 et 2 | |
Yes | 8.2 ± 0.4 | 61.3 ± 3.1 | 4 | ||
RR (20%)/EtOH (80%) | No | 2.4 ± 0.0 | 0.0 ± 0.0 | 1 | |
Yes | 2.5 ± 1.3 | 8.7 ± 9.9 | 2 |