Table 4 Density of sapwood samples after being buried for 2 years

From: Analysis by next-generation sequencing of bacterial communities in Japanese cedar logs buried for 2 years for ground improvement

Log code

Section

Sapwood

Density (g/mL)

A

Upper

0.39

Middle

0.40

Lower

0.39

B

Upper

0.33

Middle

0.37

Lower

0.35

C

Upper

0.32

Middle

0.34

Lower

0.33

D

Upper

0.31

Middle

0.32

Lower

0.31

E

Upper

0.32

Middle

0.30

Lower

0.31